Differential Scanning Calorimetry (DSC)

In differential scanning calorimetry (DSC) the difference in heat flow between sample and reference sensors is measured as a function of temperature.  DSC can be used to study phase transitions such as melting, crystallization, cold crystallization or glass transition, as well as heat capacity.  This versatile thermal analysis technique may be used to study cure and crystallization kinetics, and to determine material purity.  It provides information on processing effects and material fingerprinting characteristics.  Numerous DSC techniques are offered by Arkema Analytical Solutions.  These include:

  • Standard DSC
  • Pressure DSC
  • Modulated DSC

Standard DSC

At Arkema Analytical Solutions our DSC units are configured to operate over a temperature range from -170°C to 600°C, although measurements up to 725°C may be performed.  Samples may be solids or liquids.  Different pan types are available, including aluminum, hermetic, graphite, and copper.  In general DSC provides:

  • Material fingerprinting
  • Phase transition definition, including:
    • Melting point
    • Glass transition
    • Curie point
    • Crystallization
    • Phase diagrams
    • Mesophase transitions including liquid crystals
  • Melting point depression analysis
  • Heat of fusion
    • Degree of crystallinity
  • Curing
  • Cure kinetics
  • Avrami kinetics for crystallization
  • Decomposition analysis
  • Purity determination

Pressure DSC (PDSC)

Pressure DSC, which measures differences in heat flow between sample and reference sensors at increased pressure, is useful for studying decomposition and oxidative stability.  Analysis can be done in ramping mode to determine the oxidation onset temperature or isothermally to determine the oxidation induction time.  We can accommodate pressures up to 1000 psi under nitrogen or oxygen, with operation from ambient temperature to 600°C.  Other gases can be used such as carbon dioxide.  Under pressure boiling points may be elevated above decomposition points.  PDSC is useful in studying:

  • Oxidative stability
    • Oxidative onset time (OOT)
    • Oxidative induction time (OIT)
  • Decomposition

Modulated DSC (MDSC)

Modulated DSC (MDSC) allows the separation of complex overlapping thermal events that may occur in the heat flow. This is accomplished by imposing a temperature sine wave on a standard linear or isothermal temperature program to decouple the response that is rate dependent from the total conventional heat flow response.  The response that is not rate dependent can be determined by subtraction of the rate dependent response from the total heat flow.  The total sample responses is thus separated into two components:

  • Reversing
  • Non-reversing

The reversing or rate dependent component includes events that are related to the heat capacity, such as the glass transition.  Use of MDSC can be used to isolate the glass transition even when it is complicated by other overlapping thermal events, for example to identify:

  • Glass transition obscured by an aging peak
  • Glass transition separated from a cure exotherm, primarily for epoxy cures
  • Glass transition followed by decomposition

The non-reversible component includes effects due to time dependent kinetic events.  These include:

  • Polymer aging
  • Loss of solvent or water
  • Cold crystallization
  • Curing exotherm